It looks to me like their Screen Printer is doing a poor job of under stencil wiping, leaving solder paste on the underside of the stencil that gets transferred to the gold areas on the edge of the pcb. During reflow, the small balls of paste flow into nice circles. Not all stencil wiping paper is created equal. Steven E. Herring Engineering Manager Pennatronics 75 Technology Drive California, Pa 15419-0638 P 724-938-1800 x 214 F 724-938-1809 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of John Foster Sent: Tuesday, July 29, 2014 12:13 PM To: [log in to unmask] Subject: [TN] Trying to figure out possible mechanism for contamination We have been seeing a problem recently on several different CCA'S that we are having assembled. The boards are ENIG with plug and plate. The assembly shop is assuring us that these gold areas are being Protected during the entire assembly process with kapton tape. I was thinking it was flux splatter since the areas are always almost perfectly circular. The locations are very random and range from nothing to what is in the picture. Is there any other mechanism that might be causing this? On our next run I am going to go to the shop To witness the taping. But I was curious if maybe it's some other cause. Mr. Gregory was kind enough to post a picture. http://stevezeva.homestead.com/spots.jpg Any thoughts would be appreciated Thank You John Foster L3 Communicatons Confidentiality Notice: The information contained in this message is intended only for the use of the addressee, and may be confidential and/or privileged. If the reader of this message is not the intended recipient, or the employee or agent responsible to deliver it to the intended recipient, you are hereby notified that any dissemination, distribution of copying of this communication is strictly prohibited. if you have received this communication in error, please notify the sender immediately. Warning: This document may contain technical data within the definition of the International Traffic in Arms Regulation (ITAR) and is subject to the export control laws of the U.S. Government. Transfer of this data by any means to a foreign person, whether in the United States or abroad, without an export license or other approval from the U.S. Department of State, is strictly prohibited ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________