We have recently discovered some CCA's with a distinctive, transparent blue color on the solder joints. Viewed perpendicular to the solder joint surface, surface looks normal. The solder surface appears blue when viewed at an angle. I see no residues at up to 30x magnification. Boards were wave soldered using Sn63Pb37 solder with ORH1 flux, then in-line water washed with a low concentration of a saponifier as one of our common assembly processes. Any ideas of what the condition is or what caused it? Dick Krug, CSSBB, CSMTPE Lead Process Engineer Sparton Brooksville, LLC 30167 Power Line Road Brooksville, FL 34602-8299 p (352) 540-4012 (Internal Ext. 2012) [log in to unmask] ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________