Fellow TechNetters: Has anyone use the above stated product in a PWB/PCB cross section to highlight cracks/fractures. Sometimes can be used to substitute Dykeem Steel rule dye. Victor, ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________