Is thisa point to point machine? The temperature of the nozzle will be less than 325 at the top of the meniscus, depending on diameter. Are you soldering at over 10mm/s? ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________