Just out of curiosity, what are the problems with the partial plating as long as the metal isn't connected to anything? Is there a high voltage potential across the mounting holes? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Henry Rekers Sent: Tuesday, June 10, 2014 5:32 PM To: [log in to unmask] Subject: Re: [TN] Plating in non-plated holes - again That's the secondary drill process....not allowed in our specification. ____________________________________________________________________________ _________ Henry Rekers P. Eng | Schneider Electric | Global Supply Chain | Senior Manufacturing Engineer Phone: +1-250-652-7100 ext. 7510 | Toll Free: +1-866-466-7627 ext. 7510 | Fax: +1-250-544-2390 | Email: [log in to unmask] | Site: www.schneider-electric.com | Address: 2195 Keating Cross Road, Saanichton, BC, Canada, V8M 2A5 *** Please consider the environment before printing this e-mail From: Steven Kelly <[log in to unmask]> To: <[log in to unmask]>, Date: 06/10/2014 01:54 PM Subject: Re: [TN] Plating in non-plated holes - again Sent by: TechNet <[log in to unmask]> The supplier could drill these after ENIG - no violation to any specification. My 2 cents. Steve Kelly -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Henry Rekers Sent: June-10-14 4:36 PM To: [log in to unmask] Subject: Re: [TN] Plating in non-plated holes - again I agree, we do not allow secondary drilling on the first pass for registration issues. We would allow rework, but not as a practice, and our concern would be the tolerance on the hole, both registration and diameter. Could you point me out in 6012 where copper smear is not allowed? I couldn't find that. Thanks. ____________________________________________________________________________ _________ Henry Rekers P. Eng | Schneider Electric | Global Supply Chain | Senior Manufacturing Engineer Phone: +1-250-652-7100 ext. 7510 | Toll Free: +1-866-466-7627 ext. 7510 | Fax: +1-250-544-2390 | Email: [log in to unmask] | Site: www.schneider-electric.com | Address: 2195 Keating Cross Road, Saanichton, BC, Canada, V8M 2A5 *** Please consider the environment before printing this e-mail From: "Stadem, Richard D." <[log in to unmask]> To: <[log in to unmask]>, Date: 06/10/2014 12:43 PM Subject: Re: [TN] Plating in non-plated holes - again Sent by: TechNet <[log in to unmask]> While secondary drilling prohibitions do apply to drilling of the original holes after plating, they were not intended to apply to rework of the original holes which were drilled as primary (prior to plating) as long as the rework does not result in the hole being out of tolerance, either in hole diameter or location from datum registration point X0, Y0. Remember, rework means returning the original non-conforming characteristic to meet all applicable requirements. If they ended up with plating inside pre-drilled holes that is not supposed to be there, how would the fabricator then rework those holes to meet the fabricated print requirements if a strict prohibition of secondary drilling were applied? Does that mean I cannot take a dental pick and lightly scrape away a copper sliver after plating is completed? I am not talking about increasing the hole size, just using the same size bit (or etchant) to clean out any excess copper. Just call it touchup. The limitation of no secondary drilling was intended to prevent mis-registration and exposed inner layer copper and smearing, as you pointed out. But cleaning the extraneous copper from the holes already drilled is not likely to cause any mis-registration at that later step. Per 6012, any copper smear inside the unplated holes is considered a defect condition. It does not say "Well, maybe a wee widdle bit is OK." -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Tuesday, June 10, 2014 1:38 PM To: [log in to unmask]; Stadem, Richard D. Subject: RE: [TN] Plating in non-plated holes - again I know I am late chiming in, but how are non-plated through holes not secondary drilling requirements? Your drawing requirement for NPTH would supercede any fabrication specification. Or am I wrong? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Tuesday, June 10, 2014 11:35 AM To: [log in to unmask] Subject: Re: [TN] Plating in non-plated holes - again Secondary drilling of holes already drilled is not secondary drilling, however. It is rework. Rework of defects that should have been found and fixed in the first place. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Henry Rekers Sent: Tuesday, June 10, 2014 10:52 AM To: [log in to unmask] Subject: Re: [TN] Plating in non-plated holes - again I'd love to do that, but our specification demands no secondary drilling. My guess is due to past registration issues. ____________________________________________________________________________ _________ Henry Rekers P. Eng | Schneider Electric | Global Supply Chain | Senior Manufacturing Engineer Phone: +1-250-652-7100 ext. 7510 | Toll Free: +1-866-466-7627 ext. 7510 | Fax: +1-250-544-2390 | Email: [log in to unmask] | Site: www.schneider-electric.com | Address: 2195 Keating Cross Road, Saanichton, BC, Canada, V8M 2A5 *** Please consider the environment before printing this e-mail From: Brian Ellis <[log in to unmask]> To: TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask], Date: 06/10/2014 08:38 AM Subject: Re: [TN] Plating in non-plated holes - again Drill after ENIG Brian On 10.06.2014 18:26, Henry Rekers wrote: > Hey there technetters. A while back, I sent a message about enig plating > contamination in NON-plated holes. I've bounced it back to the board > shop saying that it is unacceptable, but they claim it is due to 6012 > 3.5.2 > I also think it's unacceptable in the 4552 spec. The design > documentation clearly states non-plated. It's not plated, just partially > plated. > > Any advice? > > Thanks. > ____________________________________________________________________________ _________ > > > Henry Rekers P. Eng | Schneider Electric | Global Supply Chain | > Senior Manufacturing Engineer > Phone: +1-250-652-7100 ext. 7510 | Toll Free: +1-866-466-7627 ext. > 7510 | Fax: +1-250-544-2390 | > Email: [log in to unmask] | Site: > www.schneider-electric.com | Address: 2195 Keating Cross Road, > Saanichton, BC, Canada, V8M 2A5 > *** Please consider the environment before printing this e-mail > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ________________________________ This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________