Victor I do not think that material is too common. We do nothing but CC and I have never had a customer ask for this material. Who is the manufacturer? Lloyd Duso Diamond-MT Plant Manager (814) 535-3505 www.Diamond-mt.com On Fri, Jun 20, 2014 at 8:44 AM, Victor Hernandez < [log in to unmask]> wrote: > Fellow TechNetters: > > I have not received many responses to my conformal coating inquiry, > ACCL-53T. Perhaps someone can share parameters associated with the > process such as application equipment, spray nozzle, thickness, Drying, > coverage, etc. Is there an associated IPC Standard that I can review? > I would very much appreciate any information you can share. > > Victor, > > From: Hernandez, Victor G > Sent: Wednesday, June 18, 2014 8:03 AM > To: Stadem, Richard D.; TechNet E-Mail Forum > Cc: Hernandez, Victor G > Subject: RE: Conformal Coating, ACCL-53T > > Good response for SAFETY, but searching for something more constructive > with regards to the above stated product.. > > Victor, > > -----Original Message----- > From: Stadem, Richard D. [mailto:[log in to unmask]] > Sent: Tuesday, June 17, 2014 3:47 PM > To: TechNet E-Mail Forum; Hernandez, Victor G > Subject: RE: Conformal Coating > > Yes, acceleration to 53 mph, tops, has always been a safe way to drive. > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez > Sent: Tuesday, June 17, 2014 3:01 PM > To: [log in to unmask]<mailto:[log in to unmask]> > Subject: [TN] Conformal Coating > > Fellow TechNetters: > > Anyone out there has experience with ACCL-53T? > > Victor, > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > <mailto:[log in to unmask]> > ______________________________________________________________________ > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________