Hi Jim- If you already have a Pb-free process, then using BGA's should go pretty smoothly because many observed problems are due to trying to reflow a Pb-free BGA with SnPb paste. This can be done very reliably, but takes some tweaking and experience. Since you can't directly see the joints, Xray is one option to do some kind of quality control kind of similar to normal microscope based inspection. But it is not nearly as good since Xrays can't see cracks. Yeah, they can see voids, but most voids look worse than any reliability degradation they cause. Inspect the heck out of the perimeter joints. Usually the interior ones look the same. Sometimes a tiny front-silvered mirror is needed to see underneath the parts. If you go down to smaller geometries (BGA pitch 0.7 or less), you will see lots more problems, just like going from 0603 to 0402 to 0201..... Wayne Thayer -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Jim West Sent: Monday, May 05, 2014 10:26 AM To: [log in to unmask] Subject: [TN] Production with BGA's Hi everyone, A happy Monday to you all! How many of you have experience with BGA's? We are looking at possibly having new designs that require BGA's. I have never ran, nor has my currently company, ran a process with BGA's and I'm trying to get my hands around everything needed to be successful. I believe my biggest concern will be the soldering process (material and process) and inspection afterwards. I feel pretty confident my paste printer, pick and place and reflow process will be capable of handling the BGA process based on feedback from the equipment manufacturers for those machines. I know this is a very broad question, but what do you guys think my focus should be on based on your experience? I have some time to prepare, so any feedback will be greatly appreciated. One specific question I do have is, will I need 100% X-Ray inspection? Thanks, Jim ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________