I agree, I thought flux when I was the image. Question: If it was RMA flux what kind of failures can that flux reasonably lead to? (Sorry for the Lead pun) Thanks, Bob K. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Friday, May 30, 2014 2:46 PM To: [log in to unmask] Subject: Re: [TN] Component Lead Oxidisation I cannot say for absolute certainty from just looking at the pictures, but it sure does look like RMA flux deposits from the tinning process that were not washed off completely. I can see the line of demarcation where it appears the tinning solder stopped just behind the flux. Because the flux rides up the component lead when the component is immersed into the molten solder, it tends to collect at the inside bend of the lead of ICs like this. For mission critical applications, I would be concerned. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Friday, May 30, 2014 1:34 PM To: [log in to unmask] Subject: Re: [TN] Component Lead Oxidisation Hi Wee Mei, I just want to apologize for not getting this posted sooner. I first saw your message on my phone and then got distracted by a bunch of other things and just forgot about getting your photos posted until you asked me about them. I have them posted now: http://stevezeva.homestead.com/WeeMei_1.jpg http://stevezeva.homestead.com/WeeMei_2.jpg Is this a ceramic part? It looks like to me that some of the part encapsulate bled out beneath the lead shoulder and the lead did not get plated. Steve -----Original Message----- Steve, I was looking at a batch of lead-formed part and noticed oxidisation or whatever you call them at the junction of the leads and component body. This oxidisation is only found at the bottom side of the component. I look at the raw part (before the leads are form) and found some of them having the same issue. I need your assistance to post this file for the following advices. 1) If this is not oxidisation, what is the correct term for it? 2) How serious is this "oxidisation" as the parts are used in mission critical operation. 3) What is the cause of such "oxidisation"? Regards, ~wee mei~ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________