In God we trust, all others bring micro-sections. Richard Stadem -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Sent: Wednesday, April 02, 2014 8:05 AM To: [log in to unmask] Subject: Re: [TN] PWB Microsection Report - Photos The only time I ever ask for microsections or even photos of microsections is for vendor certification or if we have, or suspect, an issue. Once I have validated a vendor and have some level of trust, there's no need for me to have the sections. A good fab shop has more at stake than I do in keeping the processes under control. If I didn't trust them enough to need to see the sections personally, I wouldn't use them. Pete ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________