Hi Guys, Anyone to know if the material of housing of connector is LCP, if can endure reflow process? Since we need rework some boards with wrong component for res we don't want to remove those press fit connectors. Lyon yuan ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________