Maybe, depends on actually material. Some LCP's will stand 290C. Test scrap part or assembly first to verify that it can stand it. Would not want to scrap a batch of PCA's because process was not verified first. Larry Dzaugis ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________