Hi Victor, It's a VERY bad thing to see even a partially lifted pad. IPC is talking only about visual, but in. MANY cases it won't be detectable during visual. Regards, Vladimir, SENTEC Sent from my BlackBerry 10 smartphone on the Rogers network. Original Message From: Victor Hernandez Sent: Wednesday, March 12, 2014 1:40 PM To: [log in to unmask] Reply To: TechNet E-Mail Forum Subject: [TN] PWB, pad lifting Fellow TechNetters: Is there any additional criteria for pad lifting others than IPC-A-610D sections 10.2.9.2? Is this for Time Zero and/or post reliability testing> Victor, ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________