Some years ago A customer buddy showed me a tin of conformal coating with a wrap on paper label. He then peeled the label off and revealed a label printed directly on can. This was for gloss yacht varnish. So it goes to show it "does what it says on the tin" -a well known advert for said varnish in UK - no matter who writes it. Its entirely possible that the use of this stuff relates to a time when board coatings finishes were not necessarily specially formulated but came from the industrial world. This stuff could have been specced in then and survives now as no one knows how to write a test regime to enable evaluation of more conventional products. That sort of situation is more common than is admitted. Have often supplied obsolete, sometime ineffective by modern criteria, products as demanded by customer for legacy products as the cost of re-approval far outweighs the cost of getting a special mix of ancient stuff made. OR it could be a spell checker typo! OR they are not using current drawing issue. OR who knows.. Regards Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Thursday, February 27, 2014 3:31 PM To: [log in to unmask] Subject: Re: [TN] Floor coating as PCA coating? No. But I have never heard of coating them with Hirschfield's Fiberglass Marine Varnish, either. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Thursday, February 27, 2014 8:56 AM To: [log in to unmask] Subject: [TN] Floor coating as PCA coating? Morning all, Silly question for the day; have any of you ever heard of using Bio-guard 251 floor coating to coat boards? Just asking is all... Steve ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________