Hmm I think I would like to know what their wiping procedure is and what they are hoping to achieve by doing it before making any firm comment. Naturally nothing has changed in your place or theirs, but something has if this has just started to appear. I would start from the premise that the boards can be no cleaner than the last thing that touched them. Unless the acetone is being allowed to flush off the board the probability is that they are making the boards dirtier. If there is anything in the acetone or on the board and it dries in place then the board will be no cleaner than it was before (the soil might be redistributed slightly) and anything in the acetone or on operators gloves will be left on board. If they are applying the acetone to the wipe by holding it against the bottle then anything in the wipes will gradually accumulate in the bottle. Quite likely they are just seeing a surface effect as you would get on any shiny surface wiped over like this. Think of cleaning a mirror. So it could be technique or the acetone is dissolving something from the wipe or softening the resist slightly. OR your boards are contaminated from packaging say and they are seeing partial removal. In this respect the boards could be ionically clean as measured by zero ion tester, but theoretically could have non ionic contamination. So a lot of what ifs and maybes at this point. Regards Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert DeQuattro Sent: Thursday, February 20, 2014 5:00 PM To: [log in to unmask] Subject: [TN] Acetone as a cleaning agent for PCBA's I have a customer that uses acetone to wipe down their PCBA's upon receipt. The assemblies we make for them are cleaned using a closed loop aqueous board washer then sampled for cleanliness with our zero-ion tester per J-std-001E guidelines. Recently this customer commented that boards appeared dirty upon cleaning with the acetone. Does anyone have any thoughts on this acetone cleaning process. Thanks, Bob ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________