Richard Stadem refers to wetting. The inference is that basic cause for QFN voiding. So we need evidence. Either epidemiological or a controlled experiment-- lead-free solder vs. good old eutectic vs. Lockheed Space nano-copper solder vs. copper plated vias (Occam). Why not a goal of eliminating all QFN voids instead of endless discussions about acceptable percentages? ----- Forwarded Message ----- From: "Stadem, Richard D." <[log in to unmask]> To: [log in to unmask] Sent: Monday, December 23, 2013 9:04 AM Subject: Re: [TN] IPC-A-610E, Voids in Thermal exposed pad of QFNs Nobody has responded to the fact that you cannot validate you actually have surface-to-surface wetting in the non-voided areas of QFNs and other SMT components with belly pads. The point I am trying to make is that QFNs really should not be used in hi-reliability devices. I know they are, but they present so many issues, and chief amongst them is cases like Reuven's, where a total amount of voiding of 25% maximum is required by his customer. There is no way to validate compliance to that requirement. The entire surface of the board pad could be covered with solder with no voiding visible in the X-ray, but none of the solder may actually be wetted to the bottom of the part. I have seen this happen many times; I was called in to determine what the reliability issue was with some QFNs overheating, and others not, and the client was puzzled because the ones that failed did not show any evidence of voids, they were completely opaque. They did not show any evidence of voiding because there was little or no wetting to the bottom of the QFN, only to the board pad, therefore no heat-sinking whatsoever. Voids only appear on belly pad solder joint X-rays if at least some of the solder is wetted to both the bottom of the part and to the pad on the PWB. From this experience, if I see a QFN belly pad solder joint without any voids at all, I immediately suspect there is no solder contact whatsoever, not the opposite. To me, voiding manifest in the X-rays of QFN solder joints is a good thing, as it indicates solder wetting took place on both surfaces. Now, if components fail because the amount of voiding is greater than 25% and you cannot guarantee your process will always provide less than 25% voiding, that is a design issue, not a process capability issue. Design engineers should take note of that. I would bill extra for the rework that is going to happen to meet that particular requirement. From: Reuven Rokah [mailto:[log in to unmask]] Sent: Monday, December 23, 2013 10:04 AM To: Stadem, Richard D. Cc: TechNet E-Mail Forum Subject: Re: [TN] IPC-A-610E, Voids in Thermal exposed pad of QFNs Hi Richard, If you design the thermal pad by dividing its area to small thermal pads you will improve the air escape possibility during the soldering process, reduce the voids creation and increase wetting. Same you have to design the stencil and its thickness accordingly. Still I am recommending to add requirements for the Power QFN voids. On Mon, Dec 23, 2013 at 5:30 PM, Stadem, Richard D. <[log in to unmask]<mailto:[log in to unmask]>> wrote: The amount of voiding in this type of part has to be directed as a percentage of the possible overall wetting. Some EMS assemblers purposely reduce the amount of solder volume to ensure the periphery leads fully wet (no pendulum effect) and to avoid solder balls under the part, which is a common problem with QFNs. So, if you only have wetting over 50% of the belly pad, you may need to have a reduced amount of voiding to correspond to protect the reliability of the solder connection and the thermal transfer or current carrying capacity. Instead of looking at the amount of voiding, it may be better to have a general requirement for the minimum amount of wetting. Now, having said that, how do you propose to ensure that the minimum amount of wetting is actually accomplished? Are the non-voided areas you see in the X-ray really wetted both to the bottom of the component and the top of the board pad? You cannot assume that. How do you know? Not even laminar X-ray (5DX or similar) can prove full surface-to-surface wetting beyond the "shadow of a doubt". All you see are shadows. Check this out: http://www.youtube.com/watch?v=owbgPVOQlbY -----Original Message----- From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Reuven Rokah Sent: Friday, December 20, 2013 10:18 AM To: [log in to unmask]<mailto:[log in to unmask]> Subject: Re: [TN] IPC-A-610E, Voids in Thermal exposed pad of QFNs Hi All, I started with this issue because of my customer needs (max 25% voids) and argue with the EMS (one one the biggest) that its guide lines require 40% maximum of voids. In my opinion it should be included in the IPC-A-610 such as class 1, 2, 3 and above class 3 such as 10% voids (using vapor phase), should be agreed between the two sides. On Fri, Dec 20, 2013 at 3:04 PM, David D. Hillman < [log in to unmask]<mailto:[log in to unmask]>> wrote: > Hi Joyce - sometimes we can get too technical and over think a component. > As you detailed, there can be a number of inputs to the equation but > not necessarily. We have been using the 50% maximum void rule for 5 > years on QFNs and I have only 2 cases where we had either a thermal > or grounding issue that required us to maintain a smaller voiding > percentage of the thermal pad. > > Dave > > > > From: Joyce Koo <[log in to unmask]<mailto:[log in to unmask]>> > To: 'TechNet E-Mail Forum' <[log in to unmask]<mailto:[log in to unmask]>>, > "[log in to unmask]<mailto:[log in to unmask]>'" <[log in to unmask]<mailto:[log in to unmask]>> > Date: 12/20/2013 06:45 AM > Subject: RE: [TN] IPC-A-610E, Voids in Thermal exposed pad of QFNs > > > > Correct me if I am wrong, as for the thermal goes, there are many > factors just the voiding. For example, the requirements of heat > transfer path - vertical vs side, MCM possibly will have multiple > grounds that may required isolation of heat path. If you allow 50% > voids, depend upon the thermal via path, you might missing one sector > of the MCM heat conduction path all together (if it is vertically > channeled). It is not as easy as a single number. It is a bit of > scary when the design is so far above the supply chain. > > Joyce Koo > Researcher > Materials Interconnect Lab > Office: (519) 888-7465 79945 > BlackBerry: (226) 220-4760 > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of David D. Hillman > Sent: Friday, December 20, 2013 7:36 AM > To: [log in to unmask]<mailto:[log in to unmask]> > Subject: Re: [TN] IPC-A-610E, Voids in Thermal exposed pad of QFNs > > Hi Reuven - I think that is a possible idea, however, what void > percentage > > do you suggest and what technical data/investigative studies do you > have to support the recommended void percentage? One thing to consider > is that if a workmanship topic is missing from the JSTD-001/IPC-610 > documents, it doesn't mean that the topic hasn't been reviewed. The > IPC committees work > > hard to only put workmanship criteria in the specifications that is > necessary and is supported by data. An example - the IPC-7093 BTC > committee completed extensive efforts looking at the voiding of QFN > thermal pads and found no industry consensus on a void percentage > requirement. The JSTD-001 committee therefore has not included a > maximum void percentage requirement in the 001 specification and the > IPC-610 specification shows no examples of voiding requirements of QFN > thermal pads. The workmanship criteria show in the JSTD-001/IPC-610 > specifications > > results in added costs to products and processes so the committees are > very careful to not add requirements unless there is technical > data/justification. I know a number of OEMs/CEMS who have a 50% > maximum void requirement on the QFN thermal pad unless the component > has specific thermal or electrical functional requirements. The > IPC-7093 specification has some good information on the topic of BTC > thermal pads and voids. The committees would welcome any investigative > data on the topic too. Happy Holidays! > > Dave Hillman > Rockwell Collins > [log in to unmask]<mailto:[log in to unmask]> > > > > From: Reuven Rokah <[log in to unmask]<mailto:[log in to unmask]>> > To: <[log in to unmask]<mailto:[log in to unmask]>> > Date: 12/20/2013 12:48 AM > Subject: [TN] IPC-A-610E, Voids in Thermal exposed pad of QFNs > Sent by: TechNet <[log in to unmask]<mailto:[log in to unmask]>> > > > > Hi TechNets, > > I didn't see in the IPC-A-610E any acceptability reference in regards > with the percentage of voids in solder joints of exposed thermal pads > of QFNs or other components with exposed thermal pads. > > I recommend to add it in the next revision. > > > -- > > Best Regards, > > *Reuven Rokah* > > Mobile: 972-52-6012018 > Tel: 972-3-9360688 > Fax: 076-5100674 > <http://www.rokah-technologies.com/>[log in to unmask]<mailto:[log in to unmask]> > [log in to unmask]<mailto:[log in to unmask]> > www.rokah-technologies.com<http://www.rokah-technologies.com> > > > This e-mail message is intended for the recipient only and contains > information which is CONFIDENTIAL and which may be proprietary of > RokahTechnologies. If you have received this transmission in error, > please inform me by e-mail, phone or fax, and then please delete all > of the original files and all other copies exist. > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask]<mailto:[log in to unmask]> > ______________________________________________________________________ > > > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask]<mailto:[log in to unmask]> > ______________________________________________________________________ > --------------------------------------------------------------------- > This transmission (including any attachments) may contain confidential > information, privileged material (including material protected by the > solicitor-client or other applicable privileges), or constitute > non-public information. Any use of this information by anyone other > than the intended recipient is prohibited. If you have received this > transmission in error, please immediately reply to the sender and > delete this information from your system. Use, dissemination, > distribution, or reproduction of this transmission by unintended > recipients is not authorized and may be unlawful. > > > > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask]<mailto:[log in to unmask]> > ______________________________________________________________________ > -- Best Regards, *Reuven Rokah* Mobile: 972-52-6012018 Tel: 972-3-9360688 Fax: 076-5100674 <http://www.rokah-technologies.com/>[log in to unmask]<mailto:[log in to unmask]> [log in to unmask]<mailto:[log in to unmask]> www.rokah-technologies.com<http://www.rokah-technologies.com> This e-mail message is intended for the recipient only and contains information which is CONFIDENTIAL and which may be proprietary of Rokah Technologies. If you have received this transmission in error, please inform me by e-mail, phone or fax, and then please delete all of the original files and all other copies exist. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________ -- Best Regards, Reuven Rokah Mobile: 972-52-6012018 Tel: 972-3-9360688 Fax: 076-5100674 <http://www.rokah-technologies.com/>[log in to unmask] <mailto:[log in to unmask]>[log in to unmask]<mailto:[log in to unmask]> www.rokah-technologies.com<http://www.rokah-technologies.com/> [http://royiro.weebly.com/uploads/6/3/6/9/6369812/4511319.jpg?303] This e-mail message is intended for the recipient only and contains information which is CONFIDENTIAL and which may be proprietary of Rokah Technologies. If you have received this transmission in error, please inform me by e-mail, phone or fax, and then please delete all of the original files and all other copies exist. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________