We have had a go round on this exact topic before when learned types went into the matter in some detail with references. The conclusion was pretty well as Kevin summarises: solder or pressfit but not both. Searching the archive will no doubt turn it up. Regards Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin Sent: Tuesday, December 03, 2013 4:01 PM To: [log in to unmask] Subject: Re: [TN] Press Fit Bad idea. For one thing, most all press-fit contacts have a hard gold finish. If you solder this, your solder joint will be a ripe candidate for gold embrittlement. It is a J-STD-001 requirement to remove gold prior to soldering. And tinning prior to insertion would increase lead diameter and insertion forces, likely leading to PTH damage. Second, press-fit insertion is an interference fit. There was a discussion just yesterday in TN about the criticality of getting the PCB hole spec just right for both the drill and finish sizes. The installation results in a hoop stress to the PTH. One can only imagine what can happen if you then take that to solder temperatures. Lead interference with the PTH for TH soldered applications is a no-no. My 2 cents. Kevin Glidden -----Original Message----- From: Vargas, Stephen M [mailto:[log in to unmask]] Sent: Tuesday, December 03, 2013 10:36 AM To: [log in to unmask] Subject: [TN] Press Fit All: I have a customer who is specifying a press fit connector to be soldered after the press fit operation. I've never heard of this and I was wondering if there is any quality/reliability data in the industry as to why one should/shouldn't do this. Our customer's explanation was that it would add mechanical integrity to the joints. Thanks in advance. Regards, Steve Vargas ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ This E-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return E-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________