Is that on the level? Dewey -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Hansatech Sent: Tuesday, October 01, 2013 10:42 AM To: [log in to unmask] Subject: Re: [TN] HASL question I have seen high quality horizontal hot air level which was so flat (by eye) I didn't realise it was HASL until told. I've never seen vertical HASL that flat. Regards Rex Sent by me on my iPhone. > On 1 Oct 2013, at 18:26, Louis Hart <[log in to unmask]> wrote: > > Technetters, in PCB fabrication with tin-lead final finish, is it easier to get solderable surface mount pads with a horizontal HASL machine than with a vertical HASL? I have thought horizontal would make it easier. Thanks for any insight. > > Louis Hart > Compunetics > Monroeville, PA > USA > [log in to unmask]<mailto:[log in to unmask]> > 412-858-1232 > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask] > ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________