Press-fit connectors normally formed by section of blocks and, as mentioned by Philip, it can be removed but the process is destructive to the connector. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Bavaro Sent: Wednesday, 23 October 2013 9:44 PM To: [log in to unmask] Subject: Re: [TN] Press Fit Connector replacement I had some experience.....but I have not performed this for about ten years...... I used to remove and replace press fit connectors when we would have problems with proper insertion. It required completely destroying the connector body with cutters and extracting the compliant pin by pin out of the PWB with a pair of pliers. I do not remember damage to the barrel after removal. The key was having the right amount of copper plating in the barrels. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerr, Bryan (UK) Sent: Wednesday, October 23, 2013 6:29 AM To: [log in to unmask] Subject: [TN] Press Fit Connector replacement Hi All Any views or experience of replacing press fit connectors ? I have some concerns since I would assume there would be some copper thp distortion during the first fit and this may affect the reliability of the refit ? Some internet trawling seems to show that the "compliant" design pins, where there is a slot in the centre, are more compatible with remove and replace since some of the distortion will be in the pin. It is a "compliant" type of pin in my case but could do with some assurance that this would be OK to do. Any thought / experiences appreciated Regards Bryan Kerr BAE Systems ******************************************************************** This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender. You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person. ******************************************************************** ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ________________________________ This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________