Folks, I has a similar experience in which I questioned the use of HASL or ImSn and did not receive any feedback. What is the difference between ImSn and HASL besides the volume of solder left on the pads. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer Sent: Wednesday, October 02, 2013 5:45 AM To: [log in to unmask] Subject: Re: [TN] HASL question Hi Steve- From these limited pictures, the finish looks like ImSn: On the solder sample picture, the parts of pads not wet by solder look matte to me. On the close-up of the original picture, the "tarnish" area is more likely copper being exposed as the thin layer of ImSn gets sucked into the solder joint. (ImAg does the same thing if you don't have the right profile.) If the pads on the boards "as delivered" are matte white, you're dealing with either ImSn or ImAg. But most ImAg formulations wet a lot better than most ImSn formulations because, as noted many times on this forum, Ag oxides are easy to solder to, but Sn oxides can create lots of problems. However, Ag oxides are visually trivial to detect, so if you wrap a fresh board up with a peeled hardboiled egg, then you'll know in a few hours whether the finish is ImAg. Since Pb free HASL deposits mostly Sn, it may be difficult to discern whether you're dealing with ImSn or HASL unless the finish is matte. (Bright Sn plate is usually even less desirable than matte Sn since it grows whiskers the fastest.) A cross-section should show a "considerable" thickness of Sn if the finish is really HASL (>5 microns). I can't remember if IPC specs have a minimum thickness for HASL coating--it's a finish I only use rarely. And, of course, HASL should show "puddling". An interrupted ENIG would usually have enough Ni on it that you could clearly see it in a cross-section at around 200X. And, of course, there are several analytic techniques and instruments available at external labs to see whether you are looking at Sn or Ni. Wayne -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 01, 2013 7:14 PM To: [log in to unmask] Subject: Re: [TN] HASL question Okay here's another picture. I printed a solder sample and sent it through the oven and this is what it looked like: http://stevezeva.homestead.com/SolderSample.jpg You can see all the non-wetting going on. The board was profiled and it was fine. We are using a FCT Assembly WS889 SN100C solder paste. What is even more strange is that the first side of the board looked okay, but the second side looks like in the photos, like the problem is confined to one side of the board if that's possible. The solder sample was only reflowed once, but I printed the paste on the side that was to be built last. Weird huh? I know you can't tell anything for sure just from some photos, but it's the strangest thing I've seen in a while... Steve -----Original Message----- From: Steve Gregory Sent: Tuesday, October 1, 2013 4:46 PM To: [log in to unmask]; Steve Gregory Subject: RE: [TN] HASL question Here's one picture: http://stevezeva.homestead.com/NonWetting.jpg Look at the left pad and the tarnish that you see there, does that look like tarnished nickel? This is after the board was washed. I have places all over the board that looks like this. I'll post a picture of what it looks like after I printed a solder sample with paste and sent it through the reflow over Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 1, 2013 4:16 PM To: [log in to unmask] Subject: Re: [TN] HASL question Ahhhh....it's what I figured. I think that's what happened. I'll have pictures later. Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer Sent: Tuesday, October 1, 2013 4:15 PM To: [log in to unmask] Subject: Re: [TN] HASL question No. Not unless somebody screwed up. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 01, 2013 6:11 PM To: [log in to unmask] Subject: Re: [TN] HASL question Hi all, It's funny that the HASL topic has come up today, because we just ran a board today that supposedly was lead-free HASL finished, and man it looks like crap! Question; does a PCB get nickel before it gets Lead-free HASL'ed? Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev. PhD Sent: Tuesday, October 1, 2013 2:23 PM To: [log in to unmask] Subject: Re: [TN] HASL question Hello Victor, It wouldn't solder in a first place. -- Best regards, Vladimir Igoshev. PhD mailto:[log in to unmask] SENTEC Testing Laboratory Inc. 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________