Try AST Corp out of New Hope, MN. www.ast-corp.net -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Thursday, September 19, 2013 10:49 AM To: [log in to unmask] Subject: Re: [TN] Adhesive Mix and Dispense Machinary Nordson EFD instead of Asymtek, Cox, Dispensing Technology, Glenmarc, Graco, Liquid Control Corp, Precision Valve and Automation, Henkel/Loctite, Sealant Dispensing and Engineering. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls Sent: Thursday, September 19, 2013 11:38 AM To: [log in to unmask] Subject: [TN] Adhesive Mix and Dispense Machinary Good morning all, I am looking for companies that will make equipment to mix and dispense adhesives. I have a quote from PVA, and Speedline and Camalot have declined to quote. Have not asked Nordson Asymtek yet. What other companies are there that I might approach? Thanks. Doug Pauls ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________