We see it often. The silicone adhesive may cause dewetting around the edges of the tape or tape dots. Sometimes this can be desirable to keep the coating off the masking making it easier to remove. Some coatings exhibit no dewetting what-so-ever. As Doug would say, it depends. Lloyd Duso Diamond-MT Plant Manager (814) 535-3505 www.Diamond-mt.com On Tue, Aug 6, 2013 at 9:17 AM, Stadem, Richard D. < [log in to unmask]> wrote: > Do you think the silicone adhesive on Kapton and Shercon tapes can create > a manufacturing issue during conformal coating or for sensitive electronics? > Doug, I would be especially interested in your respected input on this > question. > > This message and/or attachments may include information subject to GDC4S > S.P. 1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed > only by authorized recipients. Use, storage and transmission are governed > by General Dynamics and its policies. Contractual restrictions apply to > third parties. Recipients should refer to the policies or contract to > determine proper handling. Unauthorized review, use, disclosure or > distribution is prohibited. If you are not an intended recipient, please > contact the sender and destroy all copies of the original message. > > > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________