This announcement is for IPC-9708-CN in Chinese. The original document was released in English in December 2010.
IPC New Release:
鉴定印制板组件焊盘坑裂的测试方法 (Chinese Language)
对SMT组件定期进行机械弯曲和冲击测试,以确保它们能够承受预期的生产、搬运和最终使用条件。在弯曲和冲击测试过程中,加载于SMT组件的应变和应变率在焊点附近会导致各种失效模式。本文件提供了测试方法去评估印制板组装(PBA)材料的敏感性和关于表面贴装技术(SMT)的连接焊盘下方绝缘材料接合失效的设计。这些测试方法,包括引脚拉拔、焊球拉拔、焊球剪切测试,可以对不同的印制板的材料和设计参数进行排序和比较。全文共17页。2010年12月发布。2013年5月翻译。
预览本标准目录.(PDF文件)
Hard copy:
Member Price: $36.00
Industry Price: $72.00
IPC members may request a free single user download of a document with digital rights management of each new standard by e-mailing
[log in to unmask] within 90 days. The file is enabled to print one copy of the standard. Please note that you will receive the file from an e-mail from IHS.com. The file must be
opened within 2 business days and will LOCK to the computer of the person who OPENS the file.