Phil, This is "new build" although not built by my company. They are post-plated min. 40u" (1.02 microns) matte tin (lead free) over min. 80 u" (2.04 microns) nickel. The tin plate over nickel is probably reflowing during wave/selective/hand soldering to the PCB, but I don't know this for certain as I've not observed it personally, only the end result. Ed Popielarski Engineering Manager 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0965 Cl: 949-581-6601 https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Thursday, June 06, 2013 12:46 PM To: TechNet E-Mail Forum; Ed Popielarski Subject: RE: Dewetting on high current connector Hi Ed, Was this a solder coated blade connector? Dewetting normally applies to something that has been exposed to solder and I am not sure why a connector would get a soft metal (solder) finish. Is this a field return (can't tell if I am seeing corrosion) or freshly produced item? Phil -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski Sent: Thursday, June 06, 2013 12:00 PM To: [log in to unmask] Subject: [TN] Dewetting on high current connector Greetings fellow 'netters, I have discovered a dewetting condition on high current blade connector(s) which causes me to raise an eyebrow. I can't find any scholarly articles discussing the long term effect such an irregular surface at the material contact interface (photo located at http://stevezeva.homestead.com/Terminal_de-wetting.JPG ) will have on connection integrity at high current. This is an extreme environment automotive application with MTBF expectations in excess of 10 years. Any guidance and/or professional opinions would be greatly appreciated. As always, thanks to Steve G. for sharing his webspace with us! Ed Popielarski Engineering Manager [Description: FullLogo] 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0965 Cl: 949-581-6601 https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ________________________________ This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________