For repair of lifted pads, no matter what epoxy is used, I put a couple of pieces of ESD-safe, low-outgassing polyimide tape over the pad and then lightly clamp it down in a deep-throat (leave it alone, Dewey) C-clamp to ensure it is properly aligned. Then I put the CCA and the clamp together in the oven to cure. The tape will not adhere to the adhesive, and leaves the whole area with a nice flat shiny coating of epoxy. It also keeps the epoxy off of the surface of the pad. Armstrong C7 with hardener "W" is the best epoxy I have found for repairs of this type. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick Sent: Wednesday, May 08, 2013 12:39 PM To: [log in to unmask] Subject: Re: [TN] 2-part epoxy for pcb repair Wow amazing and timely, just got into a conversation with a fellow technician over this very subject yesterday. He was looking at the film adhesives from Circuit Technology and I prefer to use a two part rapid set epoxy, due to the stated reasons. I believe the copy we have of 7711A/7721A recommends thermally bonded adhesives. My issue is that when the land or pad is soldered to, the trace can shift or lift as the "glue" is heated. I was originally trained using Loctite super glue with a liquid activator, however again when the area is heated the bonding agent sometimes releases. I have had best results using BARCO BOND MB-165 quick set epoxy made by Astro Chemical, sets in 10-15 seconds, cures in a couple of minutes, I use their 100X product for board repair, it has longer working and cure times, on the order of 20 minutes, usually will mix in some shredded board when I need a large fill or strength and to color match. I know it isn't totally what you are looking for but may be an alternate. Pat -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Wednesday, April 24, 2013 1:43 PM To: [log in to unmask] Subject: [TN] 2-part epoxy for pcb repair Good afternoon, I am drawing an absolute blank trying to remember the 2-part epoxy that I've used in the past for PCB repair (sheesh)! Can anybody refresh my memory? The little epoxy packets from Circuit Technology Center are pretty pricey. I remember that I used something else, but can't remember what it was? Thanks! Steve Gregory ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ PG&E is committed to protecting our customers' privacy. To learn more, please visit http://www.pge.com/about/company/privacy/customer/ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________