There is an anomaly at the corner solder bump, without further x-ray tilt inspection, not sure what it is. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, April 30, 2013 4:08 PM To: [log in to unmask] Subject: Re: [TN] Pic of head-in-pillow for the site Hi Dave! Have your picture posted, it's here: http://stevezeva.homestead.com/HOP_iso1.jpg It's the corner ball, right? Steve Gregory From: [log in to unmask] [mailto:[log in to unmask]] Sent: Tuesday, April 30, 2013 12:43 PM To: Steve Gregory Subject: Re: [TN] Pic of head-in-pillow for the site Steve - please post this HOP too - same type of thing as Ed's but another example for everyone benefit: Dave From: Steve Gregory <[log in to unmask]> To: <[log in to unmask]> Date: 04/30/2013 10:56 AM Subject: Re: [TN] Pic of head-in-pillow for the site Sent by: TechNet <[log in to unmask]> ________________________________ Hi Ed! Nice image! Got it posted, it's here: http://stevezeva.homestead.com/Head-in-pillow_X-Ray.JPG <http://stevezeva.homestead.com/Head-in-pillow_X-Ray.JPG> What about the void off to the right? Is there any concern about that? Steve Gregory Process Engineer Kimco Design and Manufacturing 652 N. Five Mile Road Boise, ID 83713 (208) 322-0500 Ext. 3133 From: Ed Popielarski [mailto:[log in to unmask] <mailto:[log in to unmask]> ] Sent: Tuesday, April 30, 2013 8:58 AM To: Steve Gregory Subject: Pic of head-in-pillow for the site Hi Steve, I have a good X-Ray picture of a head-in-pillow that Leland would find helpful. If you don't mind posting it for him? Ed Popielarski Engineering Manager 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0965 Cl: 949-581-6601 https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn <https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&sp n> =0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A <https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&sp <https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&sp > n=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A> ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________