Kevin, Here my 2 cents: (1) Aero = the real one with vacuum are good, OSP not much of issue (2) Aero that sitting on the soil rotting are bad, you need to either take care at box level (seal it all) or cover the exposed copper (osp finishing the edge of the solder pads usually are not soldered - exposed copper). If you coat the board, may be not issue so much. (3) single reflow side is good = you can choose the thinner OSP. However, the shelf life and storage condition is a bit restricted. But easy to solder, if you follow the MFG instruction - compare to the thick OSP (4) there are different OSPs, immidazole - ATT's favor, benzotriazole - used to be IBM's flavor for example. Water soluble flux is aggressive, you need to watch your process window. (5) reflow might be a bit lower than your usual temperature, since it would be wet faster than ImAg I expect... just a guess. My 1.92 cents. Joyce Koo Researcher Materials Interconnect Lab Office: (519) 888-7465 79945 BlackBerry: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey Sent: Wednesday, May 22, 2013 7:17 AM To: [log in to unmask] Subject: Re: [TN] OSP processing inputs? Hi Kevin, I like OSP. When done properly, it solders great. The material is not a conductor, but it is easily pierced by a probe. It might not be good for a test point. Printing solder on the test points probably makes sense. As I understand it, Immersion Ag is protected with an OSP as part of the plating chemistry. So, there is some truth to what you read. However, the finishes are different. Silver oxide is easily reduced. In my experience the finish is more forgiving than OSP over copper. And, because it is a plating process, unlike OSP over copper, you get the assurance that the copper on the board will accept plating. Your process, optimized for ImAg should be fine with OSP. Guy -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin Sent: Tuesday, May 21, 2013 12:39 PM To: [log in to unmask] Subject: [TN] OSP processing inputs? Hi all, It looks like I will be getting some PCBs with OSP finish on them to process thru SMT. I've not yet used this surface finish, so for me there are a lot of unknowns. Some background info: 1 The PCBs will be single sided SMT, so I will not have to worry about solderability of second side reflow. 2 We are using Sn63Pb37, not lead-free. 3 We are using water soluble ORM0 paste and DI water wash only (no chemical) 4 We typically process with ImAg. 5 MIL/AERO target service environment I have read some that shelf life is reduced to around 6 months and that OSP covered pads cannot be used as test points and therefore test pads need to be solder coated. I've also read some of the conference papers which seem to indicate corrosion/environmental performance is at least as good as what we would get with ImAg. Any other suggestions / caveats ? Is there an IPC spec for this finish? Thanks in advance! Kevin ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________