They are to spec for the screw and nut. Verified. They are not necking down and devices that are not plastic maintain torque. Joyce hit the nail on the head with http://en.wikipedia.org/wiki/Stress_relaxation Ed Popielarski Engineering Manager 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0965 Cl: 949-581-6601 https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A -----Original Message----- From: Goodyear, Patrick [mailto:[log in to unmask]] Sent: Wednesday, May 15, 2013 3:02 PM To: 'TechNet E-Mail Forum'; Ed Popielarski Subject: RE: Elastic/plastic deformation of thermoplastic transistor housing Ed, Is the torque spec correct for the fastener being used? Years ago had an issue with the twelve 1/4-20 cap screws on a group transmitter covers, the cover had two 'O' rings and was torqued to a ft-lb spec when the correct spec was in in-lb, more than 3/4 of the bolts had necked to less than 2/3 their original diameter and in some instances snapped off, the cover screws when discovered were finger tight, we thought the problem was wrong material and elongation, so they changed bolts and then snapped them off, someone with a slight mechanical background picked it up. Pat Goodyear Control Technician Diablo Canyon Power Plant -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski Sent: Wednesday, May 15, 2013 8:57 AM To: [log in to unmask] Subject: [TN] Elastic/plastic deformation of thermoplastic transistor housing I have run across an interesting phenomenon and was hoping someone has done exhaustive research on it in Technet-ville. I have a TO-3PF style package (plastic power transistor with plastic tab) that has a specific torque requirement and thread-locker material (microsphere type). When the subassembly is first assembled in a fixture to align the transistors to the heatsink and hold the nut in rotational place then torqued, they are verifiably tightened correctly. Once they sit for a day or so, they are no longer tight and the screw/nut spins in situ together. To my amateur eye, it seems the thermoplastic is exhibiting elastic deformation at this point. If re-torqued again, it stays put, which seems to possibly have crossed the threshold from elastic deformation ("bending" the atomic structure) to plastic deformation ("shearing" the atomic structure). Is there any insight I can harvest before my 1:00 meeting today? Ed Popielarski Engineering Manager [Description: FullLogo] 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0965 Cl: 949-581-6601 https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ PG&E is committed to protecting our customers' privacy. To learn more, please visit http://www.pge.com/about/company/privacy/customer/ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________