Hi Pat - doesn't the use of a P-38 result in a fatal dose of lead poisoning in most instances? : - ) Dave From: "Goodyear, Patrick" <[log in to unmask]> To: <[log in to unmask]> Date: 05/08/2013 04:51 PM Subject: Re: [TN] Flux classification question NTC Sent by: TechNet <[log in to unmask]> P-38 best can opener ever invented. IMHO pat -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ahne Oosterhof Sent: Wednesday, May 08, 2013 2:41 PM To: [log in to unmask] Subject: Re: [TN] Flux classification question NTC That's why Bowie knives were invented. And if you were really handy you could open the top and bottom of the can simultaneously. Ahne. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner Sent: 08 May, 2013 09:46 To: [log in to unmask] Subject: Re: [TN] Flux classification question NTC Ah yes killed spirits, Tricene tinning flux. To me the most amazing thing about tin cans is not how they were made, but that the tin opener wasn't invented for another hundred years or so after the can. What did they do in the meantime? Best Wishes Mike -----Original Message----- From: Brian Ellis [mailto:[log in to unmask]] Sent: Wednesday, May 08, 2013 5:02 PM To: [log in to unmask] Cc: 'TechNet E-Mail Forum' Subject: Re: [TN] Flux classification question Yes indeed, Mike, your message has caused one of my synapses to fire. I had forgotten about the abortive Hughes flux. I think that the only reason that it raised interest at that time was because of the name which, in the public perception, was synonymous with good products. On reflection, it is quite astonishing that many Toms, Dicks and Harries, who knew next to nothing about soldering or flux chemistry dreamt up some flux formulations, and this goes back over a century! A very few of them made it into the mainstream! Some of them were even quite dangerous, containing such substances as aniline and hydrazine - and even methanol as solvent. Was it not Gray who said that a little learning was a dangerous thing? In other words, leave it to those who know what they're doing! A little while ago I watched a video on the history of tin cans for food preservation and it showed a reconstruction of how the earliest tin cans were made, filled with beef and sealed in the mid-1800s. Even Queen Victoria was impressed! It made me wonder how the steel was tinned and then I thought about the itinerant thinkers who tinned copper pots for households. Apparently, they used sal ammoniac in conjunction with a moleskin. I assume the copper was cleaned by the formation of an ammonium complex. However, this would not work with steel, so I assume that some acid was used, probably hydrochloric. I wonder who had the idea of adding some zinc to it? Of course, we Brits would say that it was Mr Baker! Necessity is the mother of invention! Brian On 08.05.2013 18:13, Mike Fenner wrote: > Hello Brian > I waited before answering.... > Your brainbox might not be going all the way to peak revs but it's on > all cylinders, so you are right - as usual :) I have a less secure > memory of a new wonder flux brought out by Hughes [as then was] based > on citric which was wonderful in tests but in practice had > shortcomings. This would be early/mid 90s? It was taken up under > licence by > an established flux supplier but quickly dropped. I also remember a > critique, I think on this forum so it had to be by you, explaining why > it was no good. Something to do with double bonds and insolubility. > So far as Zeva was concerned their machines were a triumph of good > German engineering over bad operating principal (they had no choice > because of patents), but so far as I recall the only reason for buying > their fluxes was > because they were part of a package. They were good for engineers to > come up > with, but were relatively easy for a specialist materials supplier to > displace. I should have said: > .... Citric acid ... has a place on the scale, but is not much used > in fluxes THESE DAYS. > > Best Wishes > > > > Mike > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis > Sent: Wednesday, May 08, 2013 1:12 PM > To: [log in to unmask] > Subject: Re: [TN] Flux classification question > > If my aged brainbox is right, ZEVA in Germany made a flux with citric > acid activator for their drag soldering machines, going back 40-50 > years. It is interesting as being a common tricarboxylic acid, > therefore quite a powerful reducing agent. It is also quite a good > chelating agent, so can "capture" difficult-to-dissolve heavy metal > salts, including both lead and tin ones, so it has a double-whammy > effect. It works best as an additive (say 20-30%) to conventional > dicarboxylic acid (e.g. adipic), rather than by itself. > > Brian > > On 08.05.2013 14:57, Mike Fenner wrote: >> HI >> The difficulty of explaining chemistry to non chemists is not to over >> explain it. This just confuses. I usually talk of strong and weak >> acids, weak being natural acids - those found in life usually with >> quite big formulas, and strong or mineral acids which are usually >> quite simple. > Using >> a scale (logarithmic) to illustrate where on the scale these things >> go and >> where fluxes would be. Also add in things from daily life which >> people are >> familiar with Fruit juices, vinegar, cola. >> Citric acid is naturally found in citrus fruits - oranges lemons - >> has a place on the scale, but is not much used in fluxes, it can have >> wash off problems. >> >> Best Wishes >> >> >> >> Mike >> >> -----Original Message----- >> From: Sue Powers-Hartman [mailto:[log in to unmask]] >> Sent: Tuesday, April 30, 2013 6:21 PM >> To: [log in to unmask] >> Subject: RE: [TN] Flux classification question >> >> Mike, >> >> I like what you wrote. While teaching J-Std001 class, I try to >> define the >> different Fluxes. Would you further define organic and inorganic? >> It is difficult to find what they are made of, tho I have been told >> that organic >> fluxes are citrus based. >> >> Thanks >> >> >> Sue Powers-Hartman >> Certified IPC Trainer: J-STD-001E, J-STD-001ES, IPC-A 600H, >> IPC-A-610E, IPC/WHMA-A-620A, IPC 7711-7721B, Killdeer Mountain >> Manufacturing >> 233 Rodeo Drive >> Killdeer ND 58640 >> 701-764-5651 ext 128 >> >> >> >> -----Original Message----- >> From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner >> Sent: Tuesday, April 30, 2013 10:45 AM >> To: [log in to unmask] >> Subject: Re: [TN] Flux classification question >> >> The term "Resin" describes a group of chemicals which includes >> natural materials such as shellac from beetles and synthetic >> materials such as epoxies. The natural material we are most familiar >> with in soldering is rosin - aka colophony - which is extracted from >> pine trees in much the > same >> way as rubber is tapped. Some of the first soldering fluxes were made from >> rosin which has nearly all the attributes needed for electronic soldering. >> It does not have quite the oxide removal properties to be totally >> satisfactory and so more active chemicals are blended with it, these >> are known as activators. The amount and type added is controlled to >> avoid too much activity which can lead to corrosion. This gave us the >> old style R (pure rosin) RMA (mildly activated and RA (fully >> activated) designations. >> You can tell the military was involved in these because mildly >> activated rosin would more naturally be abbreviated MAR rather than RMA. :) . >> These old style specs were based on composition, basically they said >> if > you >> use these materials in these proportions and they meet compositional tests >> (e.g. less than a certain amount of activator or leachable acid then >> they were considered safe. In other words pragmatic based on a few >> decades of finding out what worked and what didn't. >> Modern no clean technology requires more than just chemical and electrical >> properties, clear light residues for example and these are more >> easily met >> by using other resins. If you look at current specifications you will >> see that the no clean classification is the same for rosin or resin containing >> materials. Whether or not a flux meets modern specs is not so much > concerned >> with what is in the flux as supplied, but what the residues do after > reflow. >> So the test criteria are surface insulation resistance (SIR) of >> reflowed test pieces and so on. The post solder tests for no cleans >> were based on > how >> RMA fluxes behaved. The RE and RO in flux designations is really now >> for information only and help provide continuity from the previous >> spec regime >> and flux types to the ones we use now. [Also for those still doing >> legacy work for those requiring MIL spec fluxes.] This explanation is >> somewhat oversimplified for clarity. Hope it helps. >> >> Regards >> >> Mike Fenner >> Bonding Services & Products >> M: +44 [0] 7810 526 317 >> T: +44 [0] 1865 522 663 >> >> -----Original Message----- >> From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins >> Sent: Tuesday, April 30, 2013 2:13 PM >> To: [log in to unmask] >> Subject: [TN] Flux classification question >> >> Flux gurus, can you tell me the difference between ROLO and RELO fluxes? >> >> (Dewey, I know - the second letter is different, that isn't helpful!) >> >> Is a RELO more active or less? Or does the E mean something else? >> >> -- >> regards, >> >> Graham Collins >> Senior Process Engineer >> Sunsel Systems >> (902) 444-7867 ext 211 >> >> >> _____________________________________________________________________ >> _ This email has been scanned by the Symantec Email Security.cloud >> service. >> For more information please contact helpdesk at x2960 or >> [log in to unmask] >> _____________________________________________________________________ >> _ >> >> >> >> _____________________________________________________________________ >> _ This email has been scanned by the Symantec Email Security.cloud >> service. >> For more information please contact helpdesk at x2960 or >> [log in to unmask] >> _____________________________________________________________________ >> _ >> >> >> >> _____________________________________________________________________ >> _ This email has been scanned by the Symantec Email Security.cloud >> service. >> For more information please contact helpdesk at x2960 or >> [log in to unmask] >> _____________________________________________________________________ >> _ >> > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask] > ______________________________________________________________________ > > > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ PG&E is committed to protecting our customers' privacy. To learn more, please visit http://www.pge.com/about/company/privacy/customer/ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________