Hi Kevin, Well, I found out that quite a few of the Diss-O-pads are used here, and it's created a bit of a stir that we might not be able to use them. Do you know if adding an extra carbon bed will protect the rest of the beds longer and extend the life? Steve Gregory -----Original Message----- From: Glidden, Kevin [mailto:[log in to unmask]] Sent: Monday, April 29, 2013 2:14 PM To: TechNet E-Mail Forum; Steve Gregory Subject: RE: [TN] Bivar Diss-O-Pads and closed-loop DI systems We've been through the same exact problem. Yes, they will shorten your DI bed life. The material is a lactose binder (sugar). We actually found on some wave soldered boards they got too hot and discolored the PCB surface. We simply stopped using them and instead integrated permanent mechanical spacers into designs that use TH parts and also required spacers. We get them thru Bivar. Kevin Glidden -----Original Message----- From: Steve Gregory [mailto:[log in to unmask]] Sent: Monday, April 29, 2013 2:56 PM To: [log in to unmask] Subject: [TN] Bivar Diss-O-Pads and closed-loop DI systems Hi All, We're getting ready to change our cleaner out with a closed-loop system, and I was wondering if the use of Bivar Diss-O-Pads will harm the DI beds? I have a call into Bivar, but I thought I would ask TechNet while I was waiting. I know I'm going to have to change the water soluble mask that is currently used to one that doesn't harm the DI beds, but I don't know about the Diss-O-Pads... Steve Gregory ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________