Hi Leland, You will need a PCB that warp during reflow or use oxide balls of BGA components or very low active flux. After the cooling, the warped PCB will come bake to planar state and the is no longer active so the head on pillow may created. Reuven On Tue, Apr 30, 2013 at 4:44 PM, Leland Woodall <[log in to unmask]>wrote: > Folks, > > Can anyone out there tell me how I can intentionally create a head in > pillow defect? I want to see if our X-ray machines are capable of > detecting this condition, and if so, how repeatable they are. > > I'm sure there are several ways to do this, but I'm looking for the most > simple. > > Thanks for your help! > > Leland > > ________________________________ > > “Confidentiality Notice: > This transmission (including any attachments) may contain confidential > information belonging to the sender and is intended only for the use of the > party or entity to which it is addressed. If you are not the intended > recipient, you are hereby notified that any disclosure, copying, > distribution, retention or the taking of action in reliance on the contents > of this transmission is strictly prohibited. If you have received this > transmission in error, please immediately notify the sender and erase all > information and attachments.” > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > -- Best Regards, *Reuven Rokah* Mobile: 972-52-6012018 Tel: 972-3-9360688 Fax: 076-5100674 <http://www.rokah-technologies.com/>[log in to unmask] [log in to unmask] www.rokah-technologies.com ** This e-mail message is intended for the recipient only and contains information which is CONFIDENTIAL and which may be proprietary of Rokah Technologies. If you have received this transmission in error, please inform me by e-mail, phone or fax, and then please delete all of the original files and all other copies exist. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________