Steve, I seem to remember seeing something about it not being required to solder the center pad on some other QFNs, but I don't recall being told not to. Makes me wonder if you were talking to a designer that didn't want the pad connected electrically, but doesn't really understand the soldering process (or reliability). Ben -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo Sent: Friday, April 19, 2013 11:22 AM To: [log in to unmask] Subject: EXTERNAL: Re: [TN] QuickFilter 16-pin VQFN Customer part with small qty you might have to be - non standard. But the design sign off on the non-std and need to be prove using rel test + function test - nothing like antenna type or ground bouce, data it is OK. Normally prototype stuff. Hopefully, the leadframe is covered with solder (not exposed copper ground). Normally, QFN is high frequency or high power device, ground is essential for thermal and function, but yours might be different. (non thermal, low frequency). My 2 cents. Joyce Koo Researcher Materials Interconnect Lab Office: (519) 888-7465 79945 BlackBerry: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Friday, April 19, 2013 11:09 AM To: [log in to unmask] Subject: [TN] QuickFilter 16-pin VQFN Good morning all, I've been looking at a board that we will be building in several weeks, and one of the packages on the is a 16-pin VQFN. Part number is: QF1D512-QN-T. Datasheet is here: http://www.quickfiltertech.com/files/QF1D512%20SavFIRe%20Datasheet%20A15 .pdf I always check the datasheet to look at the recommended solder paste footprint to ensure that the stencil I spec out falls within the manufacturers recommendations. Yeah I know that sometimes the manufacturers footprint doesn't always work, but I look at it anyway for a sanity check. Well, the datasheet doesn't have one, and I sent a contact email to QuickFilter asking if they had a recommended solder paste footprint for this part and didn't receive a reply, so I called them the next day. When I spoke with them I was told that they didn't have a documented footprint for the part, but there was one thing they wanted me to know, which was to NOT print solder paste for the center pad beneath the part. "But why?" I asked, "there's a pad there in the drawing of the part...". I was told that the pad is completely non-functional, and the reason that it's there is because they didn't want to have to come up with a custom lead frame for this part, and this was the lead-frame that was "off-the-shelf" and what was used. Well, I was surprised! I mean this does make things easier for assembly by not having to worry about soldering the center pad, but this is the first time I have ever ran across something like this. Have any of you ever run across this on any other QFN parts? Have a good Friday everybody! Steve Gregory Process Engineer Kimco Design and Manufacturing 652 N. Five Mile Road Boise, ID 83713 (208) 322-0500 Ext. 3133 ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________