Guy, I don't have a paper or data sheet to reference but since the main gold embrittlement structure is Au-Sn and SAC solders are mainly Sn, I would think that SAC solders would form a brittle solder connection on a thick soft gold pad. Regards, Thomas A. Carroll, CQA, CIT, FAA ODA Unit Member Supplier Quality Engineer Boeing Defense, Space and Security - East Region Supplier Quality eFAX: 314-777-1845 Cell: 215-692-2463 Virtual Desk Phone Number: 314-545-2358 email: [log in to unmask] Go Green! Please do not print this e-mail unless necessary. NOTE: This communication may contain privileged or other confidential information. If you are not the intended recipient, or believe you have received this communication in error, please do not print, copy, retransmit, disseminate, or otherwise use the information. Also, please indicate to the sender that you have received this e-mail in error, and delete the copy you received. Thank you. EXPORT COMPLIANCE STATEMENT: "The information contained herein is or may be controlled by the International Traffic in Arms Regulations (ITAR), 22 CFR 120-130, and may not be exported, or disclosed to a foreign person, whether in the United States or abroad, without prior U.S. Government written approval" -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey Sent: Friday, March 29, 2013 2:28 PM To: [log in to unmask] Subject: [TN] solder which does ot scavenge gold Background info: We were asked to populate and assembly with a Ma-Com part, MA46H120, a GaAs Constant Gamma Flip-Chip Varactor Diode. The data sheet says: Mounting Techniques - These chips were designed to be inserted onto hard or soft substrates with the junction side down. They can be mounted with conductive epoxy or with a low temperature solder preform. The die can also be assembled with the junction side up, and wire or ribbon bonds made to the pads. Solder Die Attachment - Solder which does not scavenge gold, such as Indalloy #2 (80In-15Pb-5Ag) is recommended. Sn-Pb based solders are not recommended due to solder Embrittlement. Do not expose die to a temperature greater than 235C, or greater than 200C for longer than 10 seconds. The Indalloy #2 cost $2,222.00 for 100gm or type five solder paste. We now have another customer asking for us to solder to thick gold. They don't have a low temp requirement and asked for SnAu solder (Indalloy #182) 80Au-20Sn. . . I shudder to think what that will cost, and I don't think the part, an inductor, will survive the 300C reflow. Question: Does SAC 305 "scavenge gold"? Would it form a brittle solder connection on a thick soft gold pad? Guy ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________