For the other folks on Technet who may be listening. Do not allow the solder pot heater to remain on as you drain the last of the molten solder from the pot. Some molten solder is required to keep the pot element from overheating. When you get down to the last few pounds of solder, turn off the pot heater. The remaining solder will stay molten for a short while in the pot, usually long enough to drain the last of it out. Refer to your wave solder/selective solder machine manuals for instructions on how to drain and replenish. Some pots require solder bars to be cut up into chunks, or as you drain the solder you can pour some off into muffin pans to form small ingots. Line the bottom of the pot with these ingots or cut up chunks when you first turn the pot back on. They will quickly melt and protect the elements from going into thermal runaway. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski Sent: Tuesday, March 19, 2013 12:34 PM To: [log in to unmask] Subject: Re: [TN] Solder pot capacity of Vitronics/Soltec 6622CC Wave solder machine Steve, That's why I described the heater layout to you, so you can activate only the heaters below the current solder line. As far as getting it out, I'm almost certain there is a valve on the bottom of the pot. Risky, but essential. If I'm mistaken about the drain valve, you could always power it up on its side and let gravity assist. Ed Popielarski Engineering Manager 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0965 Cl: 949-581-6601 -----Original Message----- From: Steve Gregory [mailto:[log in to unmask]] Sent: Tuesday, March 19, 2013 10:01 AM To: Ed Popielarski; [log in to unmask] Subject: Re: [TN] Solder pot capacity of Vitronics/Soltec 6622CC Wave solder machine Thanks Ed! I'm learning more & more about this machine as the days tick down, and I haven't even seen it yet. To further complicate matters, I understand that there's a couple of hundred pounds of what maybe be SAC307 in the bottom of the pot, was told that it was analysis was this: 96.17 % Tin, .54 % copper, 3.18 % silver. The machine is intended to be used as a 63/37 machine, and getting that residual solder out is going to be a bear because I understand that the bottom of the pot has what's called a "false bottom" or welded structure inside, so it's going to be tough. I don't think I can leave the solder inside the pot with hopes of adding new solder and it will dilute what's left in the pot down enough for the solder to be within spec, in fact I'm pretty sure it won't, the silver content is especially what worries me. The previous emails from a few days ago about the tin content was with the existing wave that they have, now they have the -6622 coming in with this issue. Going to have my hands full when I get to Boise, that's for sure... Steve -----Original Message----- From: Ed Popielarski Sent: Tuesday, March 19, 2013 12:07 PM To: [log in to unmask] ; 'Steve Gregory' Subject: RE: [TN] Solder pot capacity of Vitronics/Soltec 6622CC Wave solder machine Below link says 700Kg = 1543.24. This might be lead-free, so I'd go with 1800 just to be safe. http://www.smtnet.com/mart/index.cfm?fuseaction=view_item&item_id=74987 Ed Popielarski Engineering Manager 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0965 Cl: 949-581-6601 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, March 19, 2013 8:54 AM To: [log in to unmask] Subject: [TN] Solder pot capacity of Vitronics/Soltec 6622CC Wave solder machine Hi All! Does anybody know what the solder pot capacity is of a Vitronics/Soltec 6622CC wave solder machine is with tin/lead solder in it? The reason I’m asking is because my new employer bought a used –6622 and needs to know how much solder they should buy to be able to fill the pot. They have an old electrovert now that has a 500-lb pot that we’ll be using, and I told him that wouldn’t be enough to fill the Vitronics machine. I’m thinking the 6622 holds around 1,600 –1,800 lbs., but I’m not sure... Steve ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________