Hi John, I don't remember ever seeing GB etched in the Pb-Sn eutectic. It's doable but very difficult and pretty much useless. Sometime people confuse grains with phases in the alloy. Regards, Vladimir SENTEC Testing Laboratory Inc. 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (647) 495-8727 Cell: (416) 899-1882 www.sentec.ca -----Original Message----- From: John Maxwell <[log in to unmask]> Sender: TechNet <[log in to unmask]> Date: Thu, 21 Mar 2013 20:20:05 To: <[log in to unmask]> Reply-To: TechNet E-Mail Forum <[log in to unmask]>, John Maxwell <[log in to unmask]> Subject: Re: [TN] SAC 305 etch I should have mentioned the parts are mounted and polished , I just need a chemical etch to highlight the grain boundaries similar to what is used for SnPb solder joints. Exotic techniques are not available but am looking fore something that I can put in a wet lab. John Sent from my iPad On Mar 21, 2013, at 4:37 PM, Inge Hernefjord <[log in to unmask]> wrote: > John, I used to mold the specimen in well cured two-component Araldite, do > the polishing with oil and diamond plastic discs to avoid contamination of > the solder joint with polish particles. Use specimen rotating holder.Then > wipe the stub with finest tissue to remove oil. Avoid solvents. Then > perform a couple of minutes Argon sputtering, which will enhance the > difference in hardness, Finally do microscopy with polarized light and a > variable Nomarski lens, see page 119 here: > http://bama.ua.edu/~mweaver/courses/MTE481/5_MTE481-MICROSCOPE&MODES.pdf > > There are many other methods of course, e.g. EDX element mapping mode, > which I have practiced many a times. > > Inge > > > > > On 21 March 2013 15:53, <[log in to unmask]> wrote: > >> What would a good etch be for etching SAC305 solder joints to enhance >> viewing grain boundaries? >> >> Thanks, >> John >> >> ______________________________**______________________________**__________ >> This email has been scanned by the Symantec Email Security.cloud service. >> For more information please contact helpdesk at x2960 or [log in to unmask] >> **______________________________**__________ > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________