Hi Alan Does the area of the pad match the area of the slug on the part? I would expect a 1:1 match there, if not that is a factor. We typically reduce the amount of solder we paste onto the pad for a part like this, we vary the reduction based on the presence or not of vias. Typically the problem we have historically seen is too much paste - which elevates the part and leads to bad connections on the perimeter. As for air speed of a swallow, can not advise. But I do not believe them to be capable of carrying a coconut shell. Have a great weekend. regards, Graham Collins Senior Process Engineer Sunsel Systems (902) 444-7867 ext 211 On 2/22/2013 1:23 PM, Alan Young wrote: > Hi folks, > > Please forgive me if this topic does not belong to this group. > > Let me explain my predicament. > I'm a PCB layout guy who has been asked to look at a soldering issue we are having with a 48-pin QFN 7mmx7mm [EMBER CORP - EM357-RTR], the solder slug under the part is not soldering/bonding to the PCB. The pcb footprint is made per the manufactures specification with a 5.3mm x 5.3mm solder slug pad with 9 vias finished drill size of 0.254mm. There are no soldermask features on the component or solder side over the vias. > > When the board has been reflowed, all of the 48 pins solder well but the slug has not bonded to the pcb. There are signs of solder in the slug vias on the opposite side of the board. If the part is ripped off the board, the slug is clean and solder free. > > I do not have any information about the paste screen setup or the oven profile. > > The questions I have are; > > 1 - Any ideas on why this is happening? > > 2 - Are the vias in the slug causing this problem? > > 3 - Would soldermaks capping the vias on the component side help resolve this? > > 4 - Would plugging (no capping) of the vias with epoxy help? > > 5 - Do north African sparrows fly faster then European sparrows (just seeing if anybody is reading this :-) > > I do have some photos and x-rays of the device if this will help. > > Again any help or comments would be greatly appreciated. > > Regards, > > Alan Young. > > > > This e-mail message and all attachments transmitted with it may contain legally privileged and confidential information intended solely for the use of the addressee. If you are not the intended recipient, you are hereby notified that any reading, dissemination, distribution, copying, or other use of this message or its attachments is strictly prohibited. > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________