Hi Richard To the best of my knowledge that was called up by IPC 6012. I don't know whether this is under review - but it should be (2007 = 5 year rule). I will take this matter up with the group at APEX. I suggest you apply some caution to the veracity of any data you produce, as the method really needs to be updated. The old Bellcore GR-78-CORE was superceded by method 2.6.3.7 Hope this helps Graham Naisbitt – Vice-Chairman IPC TGs: SIR / ECM; CAF & 7-11 Test methods Sub-Committee, IEC TC91 WG3 Project Leader, BSi EPL 501, UK IAG E: [log in to unmask] T: 012 5252 1500 On 7 Jan 2013, at 20:29, Richard Kraszewski <[log in to unmask]> wrote: > Can anyone tell me which IPC bare board documents references test method 2.6.3.5 to meet a minimum SIR requirement? > > Rich Kraszewski - Plexus Engineering > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________