Steve, the process is still very much alive and well with us, in fact there are some things we wouldn't solder any other way. You're right about the transfer fluids. We are using Galden HS240 and the current price is around £590 per 5kg. Overall running costs are pretty low though because the losses are not what they used to be in years gone by. Hope this is useful. Peter B. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of TechNet automatic digest system Sent: 06 December 2012 06:00 To: [log in to unmask] Subject: [SPAM?] TechNet Digest - 4 Dec 2012 to 5 Dec 2012 (#2012-313) ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________