Hi Bob, I have a question; what are the dual row connectors that you are using that rock during reflow? Dual row SMT headers usually have no problems sitting flush and perpendicular to the surface of the board as long as the footprint is correct. Is it the locating pin that they are pivoting on? I will agree with everyone about using Loctite chipbonder. I've used 3609 to keep components from moving during reflow. For instance there were some D-paks where the lay-out of thermal (or ground pad) wasn't correct for the part, and the part would center itself over the thermal pad during reflow, which would pull the leads off their pads and result in no heel fillets. A dot of 3609 was hand dispensed so that it contacted the body of the part and the PCB, and it would cure enough before the solder went liquidous during reflow to overcome the surface tension of the solder and keep the part where it was placed. The board was later spun to fix that footprint and some issues. Steve -----Original Message----- From: Robert Kondner Sent: Tuesday, December 11, 2012 1:04 PM To: [log in to unmask] Subject: [TN] Sugestions for Pre Reflow Component Adhesive Hi, Can anyone make suggestions on an adhesive to hold down components while they go through the reflow oven? I plan on using some SMT dual row .025 posts. I get them with locating pins but they still rock some. I was thinking of placing a drop of cyanoacrylate (Super Glue Gel) but that stuff gives off terrible odors at high temps. I don't think it was designed for reflow temps. Any Suggestions? Thanks, Bob K. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________