I know few of the good FAB houses strictly control RH level in the plating room for HDI (cleanroom type). Not sure if there is std or not. But you paid a bit more to get good quality boards, I mean, really good quality boards (you can sleep well at night with sweet dream without worry anything happens to your order, except earth quake or other similar event). Joyce Koo Materials Researcher - Materials Interconnect Lab Research In Motion Limited Office: (519) 888-7465 79945 Mobile: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson Sent: Tuesday, November 20, 2012 4:33 PM To: [log in to unmask] Subject: Re: [TN] FAB: Humidity Limits? oops... I'm really embarrassed! I thought I was familiar with IPC-1601 (the packaging and storage part of it anyway) which is why I was searching EVERYWHERE ELSE for fabrication info, but now I discover that IPC-1601 discusses fabrication too. I'm sorry for not doing enough homework first. but if I could ask one question about it, I only have the Final Draft of the document and it is labelled as a "Guideline", but gives real recommendations such as specific baking parameters for various situations. My question is, can (or should) board purchasers REQUIRE adherence to 1601? Can we even do that (like with notes on a drawing) if the document is just a guideline? thanks, Jack . On Tue, 20 Nov 2012 13:28:07 -0600, Jack Olson <[log in to unmask]> wrote: >After reviewing the bare board packaging and shipping recommendations in >IPC-1601 (which addresses getting the boards from the fabricator to the >assembler) the question came up about the humidity levels INSIDE the >fabricator DURING the fabrication. >Does IPC address that? Maybe I haven't had enough coffee today, but a >search for "moisture" or "humidity" in IPC-6012, IPC-A-600, etc didn't >reveal very much useful info. Are we trying to control that? Or just the >moisture level in the finished product? ___________________________________________________________________ --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________