Hi Matt, We typically use matte tin plating and the thickness range is 400 -900 microinches. Thank-you Mumtaz Bora Peregrine Semiconductor 858-795-0112 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Matthew Park Sent: Thursday, November 08, 2012 12:33 PM To: [log in to unmask] Subject: Re: [TN] tin plating I mean a typical thickness of component solder termination tin finish. From: Matthew Park Sent: Thursday, November 08, 2012 2:30 PM To: [log in to unmask] Subject: [TN] tin plating Technet, What is a typical range for tin finishes for SMT components? Is Matt tin finish thickness than Bright tin finish? Thank you for your response Park This message (including any attachments) contains confidential information intended for a specific individual and purpose, and is protected by law. If you are not the intended recipient, you should delete this message. Any disclosure, copying, or distribution of this message, or the taking of any action based on it, is strictly prohibited. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________