Conformal coat. Joyce Koo Materials Researcher - Materials Interconnect Lab Research In Motion Limited Office: (519) 888-7465 79945 Mobile: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Woolley, M. D. (M.) Sent: Tuesday, November 06, 2012 10:07 AM To: [log in to unmask] Subject: Re: [TN] Limits on flux residue From my company's experience a humid condition and sulfur (H@S, SO4-) in the atmosphere can accelerate the process. Sulfurous gasses can be found in the far east (China, India, and others) from coal fired power generating plants, oil refineries, oil pumps stations and from vulcanization of rubber). We have found that in the far east the air conditioning of the building is turned off at nights and weekends. We have found evidence of condensation on vias from the humid atmosphere being taken in by the cooling fans while the metal is still cold enough to produce local saturation and condensation. We are working with our customers to have the air conditioning on all the time, or at least dehumidify the incoming air to the point that water will not condense on the PWBs' vias at their "cool" temperature. mark -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez Sent: Tuesday, November 06, 2012 7:56 AM To: [log in to unmask] Subject: Re: [TN] Limits on flux residue Folks, A ticking time bomb for leakage and/or perhaps corrosion! How can you determine/predict when the two events will occur? What the worst case environment that will active either attribute? Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Tuesday, November 06, 2012 8:15 AM To: [log in to unmask] Subject: Re: [TN] Limits on flux residue Dave, I could not agree with you more. Excellent posting, and excellent philosophy. Too many times I hear someone say "who cares, its no-clean, perfectly safe" only to find the hard way that is not true. Not only that, but most no-clean fluxes are very effective when applied as a very, very thin sheen or veneer (less than 1 mil thick) over the BGA pads. You DON'T need gobs, more flux does not mean better wetting. Too much also means a better chance that not all of it will be heat-activated. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman Sent: Tuesday, November 06, 2012 7:27 AM To: [log in to unmask] Subject: Re: [TN] Limits on flux residue Hi Wayne - no, the JSTD-001 committee has not addressed that aspect of No Clean processing because there are a number of product use environment influences and process parameters that come into play on what is acceptable and unacceptable. Your description would lead me to believe that someone has taken extreme liberty in calling something a "no clean" process. One of the things that we have found most interesting in the implementation of a no clean process for a couple of our products is that many folks believe "no clean" is a sloppy process and you can leave flux residue anywhere on the assembly in uncontrolled quantities. But the reality is that "no clean" solder processing requires very careful control of what/how much/where you allow flux residues to exist. In my view, a "no clean" process actually is a much tighter controlled process than a process that utilizes cleaning to insure that product functionality is not impacted. Dave Hillman Rockwell Collins [log in to unmask] From: "Thayer, Wayne - IS" <[log in to unmask]> To: <[log in to unmask]> Date: 11/05/2012 05:52 PM Subject: [TN] Limits on flux residue Sent by: TechNet <[log in to unmask]> Is there a spec somewhere which limits the amount of residue allowed for no clean processing? I just saw a board where a BGA was about 70% "underfilled" by flux residue. No, this was not a flux/underfill product! A quick look at JSTD-001 Section 8 didn't seem to have specific guidance on this condition. Wayne Thayer ________________________________ Email addresses of ITT Exelis employees have changed from itt.com to exelisinc.com. Please update your favorites and contact information to reflect these changes. This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of Exelis Inc. The recipient should check this e-mail and any attachments for the presence of viruses. Exelis Inc. accepts no liability for any damage caused by any virus transmitted by this e-mail. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________