尽管达到75%,也是不可接受。
焊接终止面那面可以看到,引脚不润湿。
Dennis Song
From: TGAsia [mailto:[log in to unmask]]
On Behalf Of Justin Wu
Sent: Thursday, September 06, 2012 3:09 PM
To: [log in to unmask]
Subject: Re: [TGAsia] 焊接标准咨询
Hi Maggie,
It seems to me that the fill s/b meet the IPC-A-610E standard clause 7.3.5.1
[log in to unmask]">
Besides, you s/b consider the solder connection wetting angle as per IPC-A-610E standard clause 5—Soldering.
[log in to unmask]">
Thanks and best regards,
Justin
From: TGAsia [mailto:[log in to unmask]]
On Behalf Of Li Maggie (AE/PJ-MFG-CN)
Sent: Thursday, September 06, 2012 2:06 PM
To: [log in to unmask]
Subject: [TGAsia] 焊接标准咨询
各位大虾
现有
一问题需要想您请教:
我们的某一产品的PTH
元件在经过焊接后出现问题,切片后的图片如下图(我们公司使用的标准为IPC-A-610D III
)
请问此种现象的产品是否满足标准,如果不满足,是哪一条款不满足。
十分感谢您的回复!
[log in to unmask]">
[log in to unmask]">
Mit freundlichen Grüßen / Best regards /
诚挚问候
Li Maggie
AE/PJ-MFG-CN
Tel. +86 (512) 6767 7156
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
TGAsia是一个为业界同仁提供技术交流的平台。您可以在论坛上提出技术问题,交流行业经验,寻找供应商等。请勿发送任何招聘,广告信息。(注:对于寻求供应商的邮件,请勿回复[log in to unmask],请私下和发件人联系)。如您需要退出该邮件论坛,请直接发送邮件至
[log in to unmask] ,谢谢。
__________ Information from ESET NOD32 Antivirus, version of virus signature database 7450 (20120905) __________
The message was checked by ESET NOD32 Antivirus.
http://www.eset.com
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
TGAsia是一个为业界同仁提供技术交流的平台。您可以在论坛上提出技术问题,交流行业经验,寻找供应商等。请勿发送任何招聘,广告信息。(注:对于寻求供应商的邮件,请勿回复[log in to unmask],请私下和发件人联系)。如您需要退出该邮件论坛,请直接发送邮件至
[log in to unmask] ,谢谢。