Hi Torsten, What we do is calculate the reliability of a bare board using representative coupons (IST) by testing them at three temperatures. Typically the test temperatures are at and below Tg; 150°C 160°C and 170°C. Then we calculate the cycles to failure at your end use temperature and the number of times the computer comes on during the day, week, month etc. What we find is that every board has it's own reliability based on processing variables, the material, assembly temperature and design. We've had one instance where compromised boards had to be used. We calculated that the boards would fail in four years. The warrantee was for three years so it was decided to use the boards. The calculated failures were within 1/10 of a percent of when the boards actually failed. I think you have to test to get the information that you require. Sincerely, Paul Reid Program Coordinator PWB Interconnect Solutions Inc. 235 Stafford Rd., West, Unit 103 Nepean, Ontario Canada, K2H 9C1 613 596 4244 ext. 229 Skype paul_reid_pwb [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Torsten Hagge Sent: September 11, 2012 5:16 AM To: [log in to unmask] Subject: [TN] Reliability Hi all, has anybody a simple ALT calculation how to decrease the number of thermocycles if the thermo gradient is increased? e.g. 1000 cycles @ 10°K/min >> xxx cycles @ 15°K/min, yyy cycles @ 20°K/min ; dwell time constant Torsten Torsten Hagge Gewerbegrund 5-9 24955 Harrislee Telefon +49 (0) 461 7741-624 Telefax +49 (0) 461 7741-642 [log in to unmask] www.kristronics.de Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL Geschäftsführer Dipl.-Ing. oec. Thormod Ohm Ust-Id-Nr. DE 811182059 Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011 IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215 ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________