# Type I 99.7% gold minimum (Grades A,B or C) # Type II 99.0% gold minimum (Grades B,C) # Type III 99.9% gold minimum (Grade A only) With gold price high, you will see all different type, including a "gold color" plating with no gold from Asia (old story). Joyce Koo Materials Researcher - Materials Interconnect Lab Research In Motion Limited Office: (519) 888-7465 79945 Mobile: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Grunde Gjertsen Sent: Wednesday, August 15, 2012 8:28 AM To: [log in to unmask] Subject: Re: [TN] Hard vs. Soft gold - mil std Depends on the process but I think it's generally around 0,3% isn't it? Cheers Grunde Kitron AS Norway -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of George Milad Sent: 15.august 2012 14:14 To: [log in to unmask] Subject: Re: [TN] Hard vs. Soft gold - mil std Hard gold is alloyed with Co, Ni or Fe at about 3%. It is harder than soft gold which is pure gold. Soft gold may be electroplated, immersion gold of ENIG is also soft gold. Both soft and hard gold are solderable. Too much gold thickness could impair the solder joint reliability. Hard gold is not gold wire bondable. Best Regards George Milad Chairman IPC Plating Committee Nat'l Accts Mgr for Technology Uyemura International corp 516 901 3874 In a message dated 8/15/2012 4:36:04 A.M. Eastern Daylight Time, [log in to unmask] writes: Hi everyone, MIL-G-45204 is the military specification for electrodeposited gold plating. I hope it helps. Sefika Ozkal Piroglu Aselsan - MGEO Division -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak Sent: Tuesday, August 14, 2012 9:43 PM To: [log in to unmask] Subject: [TN] Hard vs. Soft gold It is my understanding that both hard and soft gold are electroplated. The difference is that "soft gold" is essentially pure, whereas "hard gold" is highly alloyed, often with Cobalt, to harden it. Rudy Sedlak RD Chemical Company --- On Tue, 8/14/12, Guy Ramsey <[log in to unmask]> wrote: From: Guy Ramsey <[log in to unmask]> Subject: Re: [TN] PCB finish: ENIG vs. hard gold To: [log in to unmask] Date: Tuesday, August 14, 2012, 11:32 AM I am not sure I can talk to hard or soft gold, and suitability for soldering. But, I can say that it is possible to solder to electroplated gold, which is different from Immersion Gold finish. I think some people say hard gold when they mean electroplated gold. There is a brief discussion of this in Coomb's Handbook. Guy -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin Sent: Tuesday, August 14, 2012 12:12 PM To: [log in to unmask] Subject: [TN] PCB finish: ENIG vs. hard gold Hi everyone, We have a PCB supplier who is offering "Hard Gold" as an alternate to ENIG finish, due to PCB size and processing capabilities. The application is Class 3 (mil/aero). The circuit is thin FR4 and subject to SMT reflow w/ Sn63Pb37 (non RoHS) solder alloy, and moderate flexing in end application. Can anyone offer info on the differences between the two finishes, and/or their suitability? Is there an IPC spec (or specs) that outline "hard gold"? Thanks, Kevin Glidden ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ###################################################################### Dikkat: Bu elektronik posta mesaji kisisel ve ozeldir. Eger size gonderilmediyse lutfen gondericiyi bilgilendirip mesaji siliniz. Firmamiza gelen ve giden mesajlar virus taramasindan gecirilmekte, guvenlik nedeni ile kontrol edilerek saklanmaktadir. Mesajdaki gorusler ve bakis acisi gondericiye ait olup Aselsan A.S. resmi gorusu olmak zorunda degildir. ###################################################################### Attention: This e-mail message is privileged and confidential. If you are not the intended recipient please delete the message and notify the sender. E-mails to and from the company are monitored for operational reasons and in accordance with lawful business practices. Any views or opinions presented are solely those of the author and do not necessarily represent the views of the company. ###################################################################### ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ Best Regards George Milad Nat'l Accts Mgr for Technology Uyemura International corp 516 901 3874 ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________