I used ENIG and electroplated gold as surface finishes before. Your concerns are unfounded. They are more friendlier for the board level manufacturing processes and they are better looking than HASL finish. >>> Gerald Bogert <[log in to unmask]> 8/9/2012 8:57 AM >>> August 9, 2012 Some of our OEMs manufacture PWBs using the HASL process and they use solder mask over bare copper (SMOBC) to prevent re-melting of the tin/lead from the traces during subsequent assembly level soldering operations. If SMOBC is not used, the re-melting of the solder causes blisters under the solder mask coating which can result in peeling or flaking of some of the solder mask from the traces. We have one OEM who will be manufacturing an ENIG board with solder mask. My question is with this finish, will the gold melt during assembly soldering to cause the same issue as when using HASL? Also, does anybody use SMOBC over ENIG? My understanding that it can be done but the results are not cosmetically appealing. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________