Bakelite is an old and specific brand/type of phenolic resin. I don't know what the DB 99 is. FR-2 would probably suffice, and a high-TG FR-4 would likely be better. Karen Tellefsen - Electrical Testing Alpha / 109 Corporate Blvd./ S. Plainfield, NJ 07080 [log in to unmask] 908-791-3069 From: Roger M Unwin <[log in to unmask]> To: <[log in to unmask]>, Date: 06/19/2012 10:49 AM Subject: [TN] DH 99 Bakelite laminate Sent by: TechNet <[log in to unmask]> Hi TechNet, Does anyone know if DH 99 Bakelite laminate is still available, or what a modern equivalent might be ? The drg that specifies it is dated 1973, and is for an Antenna of some type. Many Thanks -- Roger M Unwin P+M Services (R) Ltd Tel : 01706 815212 Fax : 01706 818636 http://www.p-m-services.co.uk ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ***** Please note that my E-Mail address has changed ***** Please address mail to me using our new [log in to unmask] address. ____________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please visit http://www.symanteccloud.com ____________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________