Is it on cut-off edges on the board with finest feature (or most difficult soldering feature on your product)? Joyce Koo Materials Researcher - Materials Interconnect Lab Research In Motion Limited Office: (519) 888-7465 79945 Mobile: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart Sent: Friday, June 01, 2012 3:10 PM To: [log in to unmask] Subject: [TN] pad surface analysis TechNetters, surface solderability of a batch of boards has been questioned by a customer. J-STD-003 solderability testing before the boards were shipped, and again, on spare coupons, after receipt by the customer was unremarkable, i.e., everything passed. In that context, I am wondering what analytical tools are suitable for analyzing a surface for possible contaminants or residue, in particular those which might inhibit soldering. Some searches of the archives since 28 Feb 2012 turned up no postings relating solderability and surface analysis. Thanks for any information or comments. Louis Hart Compunetics Monroeville, PA USA [log in to unmask]<mailto:[log in to unmask]> 412-858-1232 ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________