I agree with you Paul. Microvias must not have fluid filled voids. Excellent examples. Wayne Thayer -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Reid Sent: Thursday, April 12, 2012 4:04 PM To: [log in to unmask] Subject: Re: [TN] Micro Stacked Via, solid copper plating, voiding Hi Denny, This was a layer1/2 microvia that is supposed to be copper filled with a cap layer also. The microvia is on a buried via I believe but I don't remember It could be on another microvia. The section is to the center of the microvia. What we did was we preformed an IST test and this microvia failed in 19 cycles. The failure is a 10% increase in resistance. Sincerely, Paul Reid Program Coordinator PWB Interconnect Solutions Inc. 235 Stafford Rd., West, Unit 103 Nepean, Ontario Canada, K2H 9C1 613 596 4244 ext. 229 Skype paul_reid_pwb [log in to unmask] ________________________________ From: Dennis Fritz [mailto:[log in to unmask]] Sent: April 12, 2012 1:53 PM To: [log in to unmask]; Paul Reid Subject: Re: [TN] Micro Stacked Via, solid copper plating, voiding Paul, I am having a bit of a problem understanding what this construction was. Obviously layer 1 to layer 2. But there seems to have been some cap plating at layer 2. Also, the microvias seem an a very high aspect ratio. They surely were sectioned to the center of the microvia? Did the cracks you point out show up as opens or intermittents? You must have cycled these to be sectioning them, surely those are not knit lines from copper plating. Guess a little background on these would help the analysis. Thanks - Denny Fritz -----Original Message----- From: Steve Gregory <[log in to unmask]> To: TechNet <[log in to unmask]> Sent: Thu, Apr 12, 2012 9:04 am Subject: Re: [TN] Micro Stacked Via, solid copper plating, voiding Hi Paul! Sorry I didn't get your photos posted yesterday, got rather busy yesterday, but I have them posted now: http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_01.jpg http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_02.jpg http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_03.jpg http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_06.jpg http://stevezeva.homestead.com/MV_Void_with_Crystal_01.jpg http://stevezeva.homestead.com/MV_Void_with_Crystal_02.jpg Steve -----Original Message----- From: Paul Reid [mailto:[log in to unmask] <mailto:[log in to unmask]> ] Sent: Wednesday, April 11, 2012 3:06 PM To: TechNet E-Mail Forum; [log in to unmask] Subject: RE: [TN] Micro Stacked Via, solid copper plating, voiding Hi Victor, I do not know that this is covered by IPC documents or not but I know that it can be a problem. Microvia voids have typically been acceptable if you do not violate the minimum thickness requirement of the copper in the barrel of the hole. What we have is an enclosed void that has plating solution in the void by default. The void cannot be plating closed without solution being trapped in the void. This makes the void very susceptible to conductive anodic filament (CAF) type of failure if there is a crack the goes to the void. I spent years looking for that crack and finally found one. Most voids do not produce a crack but on two occasions I have found cracks into voided microvias. It is why I suggest that voids be avoided in any high end application. It is not a standard but it is my take on this problem. Voids in plated closed microvias should not be allowed is my suggestion to the 6012 committee. I have sent pictures to Steve Gregory to post on his web site. You'll note the plated closed microvias voids with cracks in the barrel on the microvia. In two pictures you will see a blue crystal that is still in the microvia that is from the plating solution. It is rare to find the blue crystal because microsectioning flushes out the blue crystals during processing. Sincerely, Paul Reid Program Coordinator PWB Interconnect Solutions Inc. 235 Stafford Rd., West, Unit 103 Nepean, Ontario Canada, K2H 9C1 613 596 4244 ext. 229 Skype paul_reid_pwb [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask] <mailto:[log in to unmask]> ] On Behalf Of Victor Hernandez Sent: April 11, 2012 11:14 AM To: [log in to unmask] Subject: [TN] Micro Stacked Via, solid copper plating, voiding Fellow TechNetters: I have searched for IPC documentation and/or Inductry Standards concerning the acceptance/guidelines for solid plated micro via voidibg. I did not locate any. Can someone confirm that and/or provided guidance as to which document covers that anomaly. Victor, ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of Exelis Inc. The recipient should check this e-mail and any attachments for the presence of viruses. Exelis Inc. accepts no liability for any damage caused by any virus transmitted by this e-mail. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________