Hi Paul! Sorry I didn't get your photos posted yesterday, got rather busy yesterday, but I have them posted now: http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_01.jpg http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_02.jpg http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_03.jpg http://stevezeva.homestead.com/MV_Void_with_Barrel_Crack_06.jpg http://stevezeva.homestead.com/MV_Void_with_Crystal_01.jpg http://stevezeva.homestead.com/MV_Void_with_Crystal_02.jpg Steve -----Original Message----- From: Paul Reid [mailto:[log in to unmask]] Sent: Wednesday, April 11, 2012 3:06 PM To: TechNet E-Mail Forum; [log in to unmask] Subject: RE: [TN] Micro Stacked Via, solid copper plating, voiding Hi Victor, I do not know that this is covered by IPC documents or not but I know that it can be a problem. Microvia voids have typically been acceptable if you do not violate the minimum thickness requirement of the copper in the barrel of the hole. What we have is an enclosed void that has plating solution in the void by default. The void cannot be plating closed without solution being trapped in the void. This makes the void very susceptible to conductive anodic filament (CAF) type of failure if there is a crack the goes to the void. I spent years looking for that crack and finally found one. Most voids do not produce a crack but on two occasions I have found cracks into voided microvias. It is why I suggest that voids be avoided in any high end application. It is not a standard but it is my take on this problem. Voids in plated closed microvias should not be allowed is my suggestion to the 6012 committee. I have sent pictures to Steve Gregory to post on his web site. You'll note the plated closed microvias voids with cracks in the barrel on the microvia. In two pictures you will see a blue crystal that is still in the microvia that is from the plating solution. It is rare to find the blue crystal because microsectioning flushes out the blue crystals during processing. Sincerely, Paul Reid Program Coordinator PWB Interconnect Solutions Inc. 235 Stafford Rd., West, Unit 103 Nepean, Ontario Canada, K2H 9C1 613 596 4244 ext. 229 Skype paul_reid_pwb [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez Sent: April 11, 2012 11:14 AM To: [log in to unmask] Subject: [TN] Micro Stacked Via, solid copper plating, voiding Fellow TechNetters: I have searched for IPC documentation and/or Inductry Standards concerning the acceptance/guidelines for solid plated micro via voidibg. I did not locate any. Can someone confirm that and/or provided guidance as to which document covers that anomaly. Victor, ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________