Hi Technet - we are beginning an effort to replace our trusty but aging Fourier Transform Infrared Spectroscopy (FTIR) system. I would like to take advantage of our Technet FTIR user community. If you are a FTIR user, please send me your recommendations and suggestions on a FTIR system (Per our Technet rules, off-line responses please). I am especially interested in the advantages/disadvantages of how your FTIR is assisting in your analysis efforts. Thanks in advance. Dave Hillman Rockwell Collins [log in to unmask] ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________